摘要:一、两种逻辑的本质区别 中文:批次式(增重 GIW):一组料斗依次向称重仓投料,称完一批、混完一批、放一批,每批独立核算。 English: Batch (gain-in-weight): hoppers feed sequentially into a weigh bin; each batch

一、两种逻辑的本质区别

称重式混料机 Gravimetric Blender


中文:批次式(增重 GIW):一组料斗依次向称重仓投料,称完一批、混完一批、放一批,每批独立核算。


English: Batch (gain-in-weight): hoppers feed sequentially into a weigh bin; each batch is weighed, mixed and discharged as an independent unit.


中文:连续式(失重 LIW):各组分料斗同时按瞬时流量连续出料,靠单位时间失重量闭环调速,料流不断。


English: Continuous (loss-in-weight): all hoppers discharge simultaneously at instantaneous rates, closed-loop controlled by weight loss per unit time, with no interruption.


二、对照要点


中文:精度——批次式单批精度高,参考 ±0.1%~±0.5%;连续式瞬时精度参考 ±0.5%~±1%,长期累计精度更好。


English: Accuracy: batch gives high per-batch accuracy (±0.1 %-±0.5 % reference); continuous gives ±0.5 %-±1 % instantaneously but better long-term cumulative accuracy.


中文:换配方——批次式换批即换,过渡料少;连续式需等料流走空,过渡料较多。


English: Recipe change: batch switches at the next batch with little transition material; continuous must flush the stream, producing more transition material.


中文:产能——批次式受称重与混合节拍限制;连续式可做大流量,适合连续产线。


English: Throughput: batch is limited by weighing and mixing cycle; continuous supports high flow for continuous lines.


中文:追溯——批次式每批一条记录,清晰;连续式按时间段记录,需时间戳对齐。


English: Traceability: batch logs one record per batch; continuous logs by time window and needs timestamp alignment.


中文:占地——批次式需混合仓,设备较高;连续式结构紧凑,可贴身安装。


English: Footprint: batch needs a mixing chamber and is tall; continuous is compact and can be installed close to the machine.


中文:适用——批次式适合注塑、多牌号小批量、色差敏感工况;连续式适合挤出、薄膜、管材、24 小时连续线。


English: Fit: batch suits injection, multi-grade small lots and color-sensitive work; continuous suits extrusion, film, pipe and 24-hour lines.


三、三个决策问题


中文:1)换牌号频率:每日换三次以上,选批次式;一条线跑一个配方一周,选连续式。


English: 1) Changeover frequency: more than three grade changes per day favors batch; one recipe for a week favors continuous.


中文:2)精度瓶颈在哪:色差敏感看单批精度,选批次;克重稳定看累计流量,选连续。


English: 2) Where is the accuracy bottleneck: color-sensitive work needs per-batch accuracy (batch); stable gram weight needs cumulative flow (continuous).


中文:3)追溯要求:客户要按批出报告,选批次式。


English: 3) Traceability requirement: if the customer wants per-batch reports, choose batch.


四、混合方案:批次 + 连续


中文:常见折中是「主料连续 + 色母与助剂失重连续添加」,或「批次配混后连续直供」。两类机型可组合,按产线节拍配置。


English: A common compromise is continuous main material with loss-in-weight masterbatch and additive dosing, or batch blending feeding a continuous line. Both types can be combined and configured to the line cycle.