色母机、失重式喂料机、称重式混料机怎么分工 Color Feeder vs LIW vs Batch Blender
一、三种设备的分工

中文:色母机(体积式/容积式):靠螺杆转速与出料口截面积估算下料量,结构简单、成本低,但实际配比会随颗粒大小、堆积密度、回料比例漂移。
English: Volumetric color feeder: estimates output from screw speed and outlet cross-section. Simple and low cost, but the real ratio drifts with pellet size, bulk density and regrind content.
中文:失重式喂料机(LIW):用称重传感器监测料斗失重速率,据此连续修正螺杆转速,适合单组分连续添加色母、助剂、填充母料。
English: Loss-in-weight feeder (LIW): load cells track the hopper weight-loss rate and continuously trim screw speed; suitable for continuous single-component dosing of masterbatch, additives and fillers.
中文:称重式混料机(GIW 批次式):多组料斗依次向称重仓投料,称完一批混一批,适合多组分整批配比。
English: Gravimetric batch blender (GIW): hoppers feed sequentially into a weigh bin, one batch at a time; suitable for multi-component whole-batch dosing.
二、对照要点
中文:计量方式——色母机按体积;失重式按瞬时重量流量;称重式按单批重量。
English: Dosing principle: volumetric by volume, LIW by instantaneous mass flow, GIW by batch weight.
中文:配比精度——色母机一般 ±1%~±3%(受物料状态影响大);失重式参考 ±0.5%~±1%;称重式批次参考 ±0.1%~±0.5%。
English: Accuracy: volumetric typically ±1 %-±3 % depending on material condition; LIW ±0.5 %-±1 % reference; GIW ±0.1 %-±0.5 % reference.
中文:适用节拍——色母机适合连续挤出在线添加;失重式适合连续线的高精度单组分;称重式适合注塑与多牌号切换。
English: Process fit: volumetric for continuous inline addition; LIW for high-accuracy single component on continuous lines; GIW for injection and frequent grade changes.
中文:换色清洗——色母机结构简单、清理快;失重式需清称重仓;称重式需清搅拌仓,换色耗时相对长。
English: Color changeover: volumetric is quickest to clean; LIW requires cleaning the weigh hopper; GIW requires cleaning the mixing chamber and takes longer.
三、选型建议
中文:只加一种色母、成本敏感、对色差宽容——选色母机。
English: Single masterbatch, cost-sensitive, tolerant of color variation: choose volumetric.
中文:连续产线、色差要求严、需按克重核算——选失重式喂料机。
English: Continuous line, tight color control, gram-weight accounting: choose LIW.
中文:一台机配三四组分、频繁换配方、要按批追溯——选称重式混料机。
English: Three to four components per machine, frequent recipe changes, per-batch traceability: choose GIW.
四、常见混搭方案
中文:方案一:称重式混料机做整批配比,下游接真空上料机直供机台,适合注塑车间。
English: Option one: GIW for whole-batch blending feeding a vacuum loader to the machine, common in injection shops.
中文:方案二:主料连续 + 色母与助剂由失重式喂料机在线添加,适合薄膜、管材、片材连续线。
English: Option two: continuous main material with LIW inline dosing of masterbatch and additives, common on film, pipe and sheet lines.
中文:方案三:体积式色母机做粗配,失重式做精修,用于预算有限的改造项目。
English: Option three: volumetric coarse dosing trimmed by LIW, for budget-limited retrofits.