PET 结晶除湿干燥一体机 Crystallizer Dryer|瓶片片材防水解干燥

日期:2026-11-20 01:11
浏览次数:22
摘要:一、产品概述 | Product Overview 中文:PET 瓶片、片材边料属于无定形状态,玻璃化温度以上会变软粘连。若直接进干燥料斗,料层会结成大块、堵料、干燥不均。所以必须先结晶,再干燥。 English: PET flakes and sheet trimmings are amorpho

一、产品概述 | Product Overview

PET 结晶干燥机 PET Crystallizer


中文:PET 瓶片、片材边料属于无定形状态,玻璃化温度以上会变软粘连。若直接进干燥料斗,料层会结成大块、堵料、干燥不均。所以必须先结晶,再干燥。


English: PET flakes and sheet trimmings are amorphous. Above the glass transition temperature they soften and stick. If fed directly into a drying hopper, the bed cakes, blocks and dries unevenly. Crystallization must come first.


中文:一体机把结晶段与除湿干燥段集成在一台设备上,中间靠热风与输送衔接,减少占地与热损失,也避免结晶后二次吸湿。


English: The combination unit integrates crystallizing and desiccant drying on one skid, linking them by hot air and conveying. It saves floor space, reduces heat loss and prevents re-absorption of moisture after crystallization.


二、工作原理 | Working Principle


中文:结晶段:瓶片在搅拌桨推动下被热风加热到 160~180℃,分子链重排形成结晶区,表面由黏变硬,结晶度参考提升到 35% 以上,料粒不再粘连。


English: Crystallizing stage: hot air heats the flakes to 160-180 °C while an agitator keeps them moving. Molecular chains rearrange into crystalline regions, surfaces harden, crystallinity rises to a reference level above 35 %, and the pellets stop sticking.


中文:干燥段:结晶料进入干燥料斗,-40℃ 以下低露点热风穿过料层,把表面与内部水分带走,含水率参考控制到 50 ppm 以下,避免挤出时水解降黏。


English: Drying stage: crystallized material enters the drying hopper, where hot air below -40 °C dew point passes through the bed, removing surface and internal moisture. Moisture content is controlled to a reference below 50 ppm to prevent hydrolytic IV drop during extrusion.


中文:整机由 PLC 按料位、料温、露点联动:结晶段供料不足自动降载,干燥段露点超限自动报警并延长干燥时间。


English: The PLC interlinks level, temperature and dew point: it derates when the crystallizer runs short of material, and alarms and extends drying time when dew point exceeds the limit.


三、核心优势 | Key Advantages


中文:结晶与干燥一体,流程短、占地小、热量不浪费

English: Integrated crystallization and drying: short flow, small footprint, no wasted heat


中文:结晶度可控,杜绝干燥结块与堵料

English: Controllable crystallinity eliminates caking and blocking in the dryer


中文:低露点深度除湿,保护 PET 黏度与制品强度

English: Low-dew-point drying protects PET intrinsic viscosity and part strength


中文:PLC 联动与数据记录,批次可追溯

English: PLC interlock and data logging for batch traceability


中文:可对接称重混料机与中央供料,形成瓶片到主机的整线

English: Interfaces with gravimetric blenders and central feeding for a complete flake-to-machine line


四、适用行业 | Application


中文:PET 瓶片再生造粒、PET 片材与薄膜、瓶胚注塑、涤纶短纤与无纺布、PLA 结晶干燥。


English: Recycled PET flake compounding, PET sheet and film, preform injection, polyester staple fiber and nonwoven, PLA crystallization and drying.