氮气除湿干燥机 N2 Desiccant Dryer|PET/PLA 光学级原料防氧化干燥
一、产品概述 | Product Overview

中文:氮气除湿干燥机以高纯氮气为干燥与载热介质,在密闭闭环中完成「加热—除湿—循环」,把料斗内的氧气含量压到极低水平,从源头断开氧化链。
English: The N2 desiccant dryer uses high-purity nitrogen as drying and heat-carrying medium. Heating, dehumidifying and circulating are performed in a closed loop, keeping oxygen content inside the hopper at an extremely low level and cutting the oxidation chain from the root.
中文:常规除湿干燥机用空气循环,空气里的氧在 150℃以上会加速 PET、PLA、TPU 的热氧化,表现为色泽变黄、黏度下降、制品发脆;氮气闭环机型主要解决这一类「干燥没问题、料却烤坏了」的问题。
English: Conventional dryers circulate ambient air. Above 150 °C the oxygen in air accelerates thermal oxidation of PET, PLA and TPU, causing yellowing, IV drop and brittle parts. The closed-loop nitrogen type solves the typical failure where drying is correct but the resin is overheated.
二、工作原理 | Working Principle
中文:氮气源(制氮机或瓶组)→ 减压稳压 → 加热器升温 → 氮气进入干燥料斗穿过料层带走水分 → 回风经除湿单元(分子筛或干燥剂转轮)脱湿 → 补入少量新氮维持氧含量 → 再加热循环。系统按露点与氧含量双闭环控制,超限自动排补。
English: Nitrogen source (PSA generator or cylinder bank) → pressure regulation → heater → nitrogen passes through the material bed in the drying hopper and removes moisture → return gas is dehumidified by the desiccant unit (molecular sieve or rotor) → make-up nitrogen keeps oxygen level low → reheat and recirculate. Dual closed-loop control on dew point and oxygen content, with automatic purge and make-up on deviation.
中文:典型控制点:露点 -40℃~-60℃、氧残留 ≤1000 ppm、料温按物料工艺设定(PET 约 160℃、PLA 约 80~100℃),具体以物料工艺卡为准。
English: Typical control points: dew point -40 °C to -60 °C, residual oxygen ≤1000 ppm, material temperature set by process card (about 160 °C for PET, 80-100 °C for PLA). Final values follow the material process sheet.
三、核心优势 | Key Advantages
中文:低氧环境,抑制高温氧化黄变,保护切片黏度与光学透过率
English: Low-oxygen atmosphere suppresses oxidation yellowing and protects IV and optical transmittance
中文:闭环循环,氮气消耗量小,长期运行成本低于开放式吹扫
English: Closed loop means low nitrogen consumption and lower running cost than open purge
中文:露点与氧含量双闭环,数据可记录导出,满足品质审核
English: Dual closed-loop on dew point and O2, with loggable data for quality audit
中文:与结晶机、称重混料机、中央供料联动,整线无人化配料
English: Linkage with crystallizer, gravimetric blender and central feeding for unmanned batching
中文:不锈钢料斗与保温层,热损失小,料温均匀
English: Stainless steel hopper with insulation, low heat loss and uniform material temperature
四、适用行业 | Application
中文:光学级 PET 片材与薄膜、PET 瓶胚、PLA 餐具与膜材、TPU 线缆护套、3D 打印耗材、医用塑胶、改性造粒。
English: Optical-grade PET sheet and film, PET preform, PLA tableware and film, TPU cable jacket, 3D printing filament, medical plastics, plastic compounding.
五、外贸标题与卖点 | Export Title & Selling Points
中文:氮气闭环除湿干燥机,适用于光学级 PET/PLA 原料防氧化干燥
English: Closed-loop Nitrogen Desiccant Dryer for Optical Grade PET/PLA Resin
中文:源头厂家|天天自动化|支持按物料与产能定制
English: Manufacturer Direct Supply | Tiantian Automation | Customized by material and capacity