六色彩虹 3D 打印耗材挤出线 6-Color Rainbow Filament Line
一、产品概述 | Product Overview

中文:彩虹耗材的难点不在挤出,而在「六个颜色点在同一根丝上按比例收敛」。六台独立挤出机分别供料,共挤模头在出口处把六股料流合成一根丝,比例与喂料量一一对应。
English: The difficulty of rainbow filament is not extrusion but converging six color streams into one strand in a controlled ratio. Six independent extruders feed separately, and a co-extrusion die merges the six melt streams into a single filament whose color ratio maps one-to-one to feed rate.
中文:整线从原料干燥、称重配比、共挤、冷却定型、测径、张力收卷到称重打包连续完成。
English: The complete line runs continuously from resin drying, gravimetric batching, co-extrusion, cooling and sizing, diameter measurement, tension winding to weighing and packing.
二、工作原理 | Working Principle
中文:六台挤出机(螺杆直径按产能配比)→ 各自经熔体过滤后进入共挤模头 → 模头内六条流道按设定角度汇合 → 出口定型为 1.75 mm 或 2.85 mm 丝 → 水槽梯度冷却(前段温水缓冷、后段冷水定型)→ 激光测径闭环反馈牵引速度 → 张力收卷。
English: Six extruders (screw diameter matched to capacity) → melt filtration → co-extrusion die where six channels merge at set angles → sizing to 1.75 mm or 2.85 mm → gradient water cooling (warm water first, cold water for setting) → laser diameter gauge closes the loop on haul-off speed → tension winding.
中文:称重混料单元为每台挤出机独立配比色母与助剂,配方切换即可改渐变节奏;测径数据与收卷张力联动,线径公差参考控制在 ±0.03 mm。
English: A gravimetric blender doses masterbatch and additives for each extruder independently, so a recipe change reshapes the color rhythm. Diameter data links to winding tension; tolerance reference ±0.03 mm.
三、核心优势 | Key Advantages
中文:六色独立供料,颜色比例由喂料量**决定,重复性好
English: Six independent feeds make color ratio a function of dosing, giving high repeatability
中文:共挤模头一次成型,免除后段拼接与二次加热
English: Single-pass co-extrusion die eliminates downstream splicing and re-heating
中文:梯度水冷与激光测径闭环,线径稳定、不椭圆
English: Gradient cooling with closed-loop gauging keeps diameter stable and round
中文:称重配比 + PLC 配方库,渐变方案可存可调
English: Gravimetric batching with PLC recipe library stores and tunes gradient schemes
中文:适配 PLA、PETG、TPU、ABS 及各类色母体系
English: Compatible with PLA, PETG, TPU, ABS and various masterbatch systems
四、适用行业 | Application
中文:3D 打印耗材生产、文创与**耗材、教学与创客耗材、特种渐变丝(温变/光变/夜光)开发。
English: 3D printing filament production, creative and gift filament, education and maker filament, specialty gradient filament development (thermochromic, photochromic, luminous).