TPD-1100 PET大有光切片结晶除湿干燥系统 1100公斤每小时 江苏仪征
适用场景|Application
大有光切片不含消光剂,透光率高,对温度与含水率都更敏感:温度偏高或停留过长容易泛黄,含水率偏高则纺丝出现气泡。1100公斤每小时配两段独立风机,结晶与除湿参数分开设定。
Bright chips contain no delustering agent and transmit more light, which makes them more sensitive to both temperature and moisture: too much heat or too long a residence yellows them, while excess moisture causes bubbles at spinning. At 1100 kg per hour two independent fans let crystallization and drying be set separately.
结构与运行|Construction and operation
预结晶段热风循环加搅拌,防止切片粘连;除湿段双塔交替吸附与再生,送风露点稳定在-40℃以下;出料走密闭管路直送纺丝料斗,减少敞口吸潮。
Hot-air circulation with agitation pre-crystallizes the chips so they do not stick; twin towers alternate in the drying section to hold the supply dew point below -40°C; discharge runs in a closed line straight to the spinning hopper.
使用要点|Operating notes
温度按牌号设定,靠停留时间脱水而不是提高温度;换批前降温清料,露点与含水率按批记录,便于追溯泛黄批次的工艺参数。
Set temperature by grade and let residence time do the drying rather than more heat; cool and clean before a batch change, and log dew point and residual moisture per batch so the process data behind any yellowing batch can be traced.
相关供货信息:PET纺丝切片深度除湿干燥系统 TPD-1600 江苏盛泽 复合短纤维切片结晶干燥线 TPD-1400 江苏仪征 PET结晶除湿干燥机 900公斤每小时 江苏海安