PET纺丝切片深度除湿干燥系统 TPD-1600 江苏盛泽
工艺位置|Process position
装在纺丝前段的结晶与除湿之间,1600公斤每小时的处理量对应盛泽一带多条长丝线并行的用量。切片进料后先完成预结晶,再进入深度除湿段,出料含水率按批次抽检留档。
Positioned between crystallization and spinning at the front end, its 1600 kg per hour throughput matches the combined demand of the parallel filament lines around Shengze. Chips are pre-crystallized on entry, then pass the deep drying section, with residual moisture sampled and logged batch by batch.
运行特点|Operation
结晶段以热风循环完成预结晶,搅拌防止切片粘连;除湿段采用双塔交替吸附与再生,送风不中断,露点保持在-40℃以下;出料经密闭管路直送纺丝料斗,减少敞口吸潮。
The crystallizing section uses hot-air circulation with agitation so chips do not stick; the drying section runs two desiccant towers alternately so supply air never stops and dew point stays below -40°C; discharge travels in a closed line straight to the spinning hopper to avoid open exposure.
选型与配套|Selection
按纺丝位数与单锭小时耗量核算,再留换批与清洗的余量;与集中供料并线时可省去中间转运,露点记录与含水率数据可按班次导出。
Size from spinning position count and hourly consumption per position, with margin for batch changes and cleaning; running it alongside central conveying removes intermediate handling, and dew-point and moisture records can be exported per shift.