文章详情

嘉兴3D打印耗材色母计量机 TMD-30|微量添加稳定配比

日期:2026-11-21 04:35
浏览次数:9
摘要:嘉兴色母计量机 TMD-30,单组微量计量 0.2~5 kg/h,配主线喂料,适合浅色耗材与功能母粒的低比例添加。 / Single-loop masterbatch doser TMD-30 for 0.2-5 kg/h low-share addition on filament lines.

色母计量机 构成图

嘉兴3D打印耗材色母计量机 TMD-30|微量添加稳定配比
Masterbatch Dosing Unit TMD-30 for Filament

浅色耗材的色母比例常在百分之一以下,这个量级上,计量机的稳定性比精度标称值更重要。
Pale filament often runs below one percent masterbatch, and at that level stability matters more than a quoted accuracy figure.

设备说明 / Equipment Overview

料斗、小直径计量螺杆与称重传感器组成单组单元,出料口直接落在挤出机进料口,不经过长距离输送,减少偏析。
Hopper, small-diameter screw and load cell form one unit feeding straight into the extruder throat without long conveying, which limits segregation.

结构与控制 / Structure & Control

按增重式结算流量,转速只作参考;换配方时输入克数或百分比,控制器自己换算螺杆转速。
Flow settles on gain in weight and screw speed is reference only; entering grams or a percentage lets the controller work out the speed.

运行与精度 / Performance & Accuracy

低比例时补料节拍会带来波动:料斗取小、补料频繁但每次量小,比大斗少补更稳;色差呈周期性时先看补料周期。
At low shares the refill cadence amplifies variation: a small hopper refilled often in small amounts is steadier than a large one refilled rarely, and periodic colour shift points at the refill cycle.

操作与维护 / Operation & Maintenance

每班清螺杆与料斗,色母受潮结块会堵小螺杆;换色时清出料口并空跑一轮,避免残料把浅色压深。
Clear screw and hopper each shift since damp masterbatch cakes and blocks the small screw, and a colour change clears the outlet and runs dry so residue cannot darken a pale shade.

参数速览 / Specifications

型号 TMD-30|喂料 0.2~5 kg/h|料斗 10 升|计量 增重式闭环|控制 触控屏 百分比或克数输入|可选 485 通讯
Model TMD-30 | 0.2-5 kg/h | 10 litre hopper | Gain-in-weight closed loop | Percentage or gram input on panel | RS485 optional

应用场景 / Applications

浅色与白色耗材的低比例调色、抗静电与爽滑母粒添加、阻燃与色母共配、再生料线的颜色补偿。
Low-share tinting of pale and white filament, antistatic and slip masterbatch, flame retardant with colour, and colour compensation on regrind lines.

选型与交付 / Sizing & Delivery

给出线径、色数、色段长度与小时产量四项即可出选型计算书,确认配置与产能;签约后按交期发运,到场安装、联动调试与操作培训,随机附手册与备件清单。
Send diameter, colour count, band length and hourly output for a sizing sheet that confirms configuration and capacity. After order we ship on the agreed date, install, commission and train, with manual and spare list.

常见问题 / FAQ

Q:色母计量机与喂料机怎么分工?
Q: How do a doser and a feeder divide the work?
A:基料走主喂料、色母走计量机,两者分开后基料流量变化不会带动色母比例;一台机器兼顾两者反而更难稳。
Base runs on the main feeder and masterbatch on the doser, so base flow changes do not drag the ratio; one unit doing both is harder to hold.

Q:比例低于千分之一还能做吗?
Q: Can it dose below one in a thousand?
A:可以但需要更小的螺杆与更高的称重分辨率,建议先做一次连续四小时的稳定性验证再定。
Possible with a smaller screw and finer weighing resolution, but verify stability over four continuous hours before committing.