尼龙化纤拉丝干燥系统 DDL-550 浙江义乌
适用场景|Application
尼龙吸湿性强,拉丝前含水率偏高时容易出现气泡丝与断头。550公斤每小时适配中小型拉丝线,也可作为试验线的前段配套。
Nylon is strongly hygroscopic, and elevated moisture before drawing shows up as bubble filaments and broken ends. At 550 kg per hour it suits small and mid-size drawing lines and can also serve as the front end of pilot lines.
工艺配合|Process fit
干燥温度控制在100℃至120℃,避免长时间高温造成氧化变色;干燥空气露点保持在-40℃以下,出料到拉丝机之间走密闭输送。
Drying is held between 100°C and 120°C to avoid long high-temperature exposure that oxidises and discolours the resin; drying air stays below -40°C dew point and the path from discharge to the drawing machine is closed.
选型要点|Selection notes
按拉丝机小时耗量与开机班次核算料斗容积;多机台场景建议加集中供料,减少人工补料带来的敞口吸潮。
Size the hopper from hourly machine consumption and shift pattern; where several machines are involved, add central conveying so manual refilling does not open the material to moist air.
相关供货信息:尼龙66纺丝除湿干燥机 DDL-600 浙江绍兴 尼龙纺丝深度除湿干燥机 DDL-800 浙江宁波 化纤拉丝切片除湿干燥机 DDL-750 江苏太仓