PET长丝纺丝除湿干燥机 DDL-1000 福建长乐
适用场景|Application
长乐一带以长丝与经编配套为主,原料牌号切换频繁。1000公斤每小时的处理量按三条线并行设计,料斗容积适中,换批清料快。
Changle runs mostly filament for warp-knitting, with frequent grade changes. The 1000 kg per hour throughput is laid out for three parallel lines, and the moderate hopper volume keeps cleaning between batches quick.
温度与露点的配合|Temperature and dew point
长丝用切片对温度敏感,干燥温度按牌号设定,靠延长停留时间脱水而不是一味升温;干燥空气露点保持在-40℃以下,出料口温度与露点同步回落,避免出料瞬间吸潮。
Filament chips are temperature sensitive, so the set point follows the grade and dehydration comes from longer residence rather than more heat; drying air stays below -40°C dew point and discharge temperature falls together with it so the resin does not re-absorb moisture at the outlet.
配套建议|Supporting equipment
与称重式混料机联动可按比例配入回料,回料比例高的场合建议前段加除尘与除铁,减少杂质对风路与露点的影响。
Paired with a gravimetric blender it can dose regrind by ratio; where regrind share is high, add dedusting and magnetic separation upstream to keep impurities away from the air path and dew point.
相关供货信息:PET拉丝深度除湿干燥机 TPD-800 广东东莞 假发丝原料深度除湿干燥机 DDL-300 河南许昌 称重式混料机 800公斤每小时 福建晋江