PET瓶胚注塑干燥系统 烟台 PDS-500|PET Preform Injection Drying System
烟台PET瓶胚注塑干燥系统 PDS-500|PET Preform Injection Drying System PDS-500
面向烟台的汽车内饰件集群。系统含预结晶段、除湿干燥段与机边输送段,按 500 kg/h 级瓶胚产量配置,干燥露点 -40~-45 ℃。
For the automotive interior parts cluster in 烟台: pre-crystallising, desiccant drying and machine-side conveying in one system, sized for about 500 kg/h of preforms with a drying dew point of -40~-45 °C.
这一条重点讲:机边输送与再污染
Focus of this page: Dried pellets re-absorb moisture in conveying; insulation and sealing of the line matter more than a bigger dryer
干燥后的切片在输送段重新吸湿,输送管路保温与密封比加大干燥机更重要。烟台的瓶胚车间在换牌号与开停机阶段,这一段较容易出批量异常。
Dried pellets re-absorb moisture in conveying; insulation and sealing of the line matter more than a bigger dryer. Preform shops in 烟台 hit this hardest when changing grade and at start-up or shutdown.
三段工艺与参数 / Three stages and figures
预结晶 150~170 ℃、搅拌防粘连;干燥 160~170 ℃、露点 -40~-45 ℃、停留 4~6 小时;成品含水控制在 50 ppm 以内,输送段保温密封。
Pre-crystallising at 150-170 °C with agitation against blocking; drying at 160-170 °C, dew point -40~-45 °C, 4-6 h residence; finished moisture kept under 50 ppm, conveying line insulated and sealed.
系统带露点、料温、料位三路显示,异常时报警而不是直接停机,便于值班人员判断。
Dew point, material temperature and level are all displayed; faults raise an alarm instead of an immediate stop, so the operator can judge.
交货与调试:烟台及周边可上门安装并带料试机,随机提供中英文工艺参数表。
Delivery: installation and trial runs with material are available in 烟台 and nearby, with a bilingual process parameter sheet.