# PET Desiccant Dryer
PET Desiccant Dryer adopts twin-tower molecular sieve desiccant technology, specially designed for hygroscopic PET pellets, rPET flakes and PET preform production lines.
Ambient air is first filtered to remove dust, then sent into molecular sieve adsorption tower, where water vapor is fully absorbed to generate constant low dew-point dry air (-40℃ ~ -50℃). The dry air is heated to 160–175℃ and evenly blown through the drying hopper filled with PET raw materials, taking away the bound moisture inside pellets after 4–6 hours constant-temperature drying.
The damp exhaust air flows back to the dehumidifier unit. The two molecular sieve towers switch automatically: one tower adsorbs moisture for drying circulation, the other one uses high-temperature hot air to desorb and discharge water outwards for regeneration. Alternating adsorption and regeneration ensures uninterrupted supply of dry hot air all day long.
This equipment can reduce PET moisture content below 50ppm, effectively avoid material hydrolysis, bubbles, haze and brittleness of PET preforms during high-temperature injection molding. Equipped with thermal insulation agitating drying hopper, it prevents PET pellets from softening and sticking at high temperature. The whole closed-loop air circuit stops dried materials from re-absorbing moisture, stable operation for 24-hour continuous production.
## 中文对照
# PET分子筛除湿干燥机
PET分子筛除湿干燥机采用双塔分子筛除湿工艺,专为易吸潮PET切片、回收rPET瓶片、PET瓶胚生产线配套。
车间空气先过滤除尘,送入分子筛吸附塔,水汽被分子筛充分吸附,持续产出-40℃~-50℃低露点干燥风;干燥风加热至160–175℃,均匀穿过装满PET原料的干燥料斗,经过4–6小时恒温烘烤,带走颗粒内部结合水。
吸走水分的湿热风回流至除湿主机,两组分子筛塔自动切换循环:一塔吸附水汽供给干燥,另一塔利用高温热风脱附水分并向外排出完成再生。吸附、再生交替运行,实现全天不间断供给干燥热风。
设备可将PET原料含水率降至50ppm以下,从根源杜绝高温注塑时原料水解,解决瓶胚气泡、发白、脆裂等不(良);搭配保温搅拌干燥料斗,防止PET颗粒高温软化结块;整机闭环风道设计,烘干后的原料不会二次吸潮,支持车间24小时连续稳定量产。