DT-500 仿粘长丝双塔除湿干燥机组 500公斤每小时 福建长乐
适用场景|Application
仿粘长丝车间以改性涤纶为主,切片吸潮后纺丝断头与毛丝增多。500公斤每小时的双塔机组两塔交替送风,露点不因再生而抬升,适合长丝线连续开机。
Viscose-like filament shops run mostly modified polyester, and moisture picked up by the chips raises breaks and fuzz at spinning. The 500 kg per hour twin-tower set alternates supply without a dew-point lift during regeneration, which suits continuous filament operation.
结构与运行|Construction and operation
两座蜂巢转轮交替吸附与再生,切换留重叠时间;料斗保温并配料位监控;出料密闭输送,减少转运吸潮。
Two honeycomb wheels alternate with an overlap at changeover; the hopper is insulated with level monitoring and discharge is conveyed in a closed line.
使用要点|Operating notes
温度按改性牌号设定,靠停留时间脱水;露点与含水率按批记录,便于追溯断头批次。
Set temperature for the modified grade and dry by residence time; log dew point and moisture per batch to trace break-prone batches.