产品中心
PRODUCT CENTER
- 联系人 : 曹镜森先生
- 联系电话 : 0769-82226193
- 传真 : 0769-82226193
- 移动电话 : 13925217478
- 地址 : ** 广东省东莞市大朗镇仙村工业区
- Email : caojingshen@126.com
- 邮编 : 523792
- 公司网址 : http://www.szdatian.net.cn
- MSN : caoshingcer@126.com
- QQ : 454992321
东莞3D打印耗材挤出整线 TPD-1200|干燥配比挤出测径收卷

东莞3D打印耗材挤出整线 TPD-1200|干燥配比挤出测径收卷
3D Printing Filament Extrusion Line TPD-1200
整线能不能稳,看的不是单机指标,而是两条闭环分开做:测径闭环管牵引,配比闭环管喂料,混在一起调,出了问题谁也说不清是哪一段。
Line stability comes from keeping two loops apart: gauging closes on haul-off, dosing closes on feeding. Mixed together, a fault can no longer be traced to a stage.
设备说明 / Equipment Overview
六段串联依次是除湿干燥、多组份配比、单螺杆挤出、两级水冷、激光测径与张力收卷;干燥段先走,露点达标再开挤出,避免开机段气泡。
The six stages run drying, multi-component dosing, single-screw extrusion, two-stage water cooling, laser gauging and tension winding; drying starts first and extrusion waits for dew point so start-up bubbles are avoided.
结构与控制 / Structure & Control
配比段与挤出段用 PLC 联动,挤出转速变化时喂料量按比例跟随;测径数据只回给牵引与螺杆,不改配比,两条闭环各管一段。
Dosing and extrusion interlock through the PLC so feed follows screw speed, while gauging data returns only to haul-off and screw, leaving dosing untouched, one loop per stage.
运行与精度 / Performance & Accuracy
线径常见控制目标 1.75 毫米公差正负 0.02 毫米,圆度同量级;测径数据保留一个班次可回看,换料换色后的稳定时间靠它缩短。
Diameter commonly holds 1.75 mm within plus or minus 0.02 mm with similar roundness, and gauging history stays readable for a shift, which shortens settling after material or colour changes.
操作与维护 / Operation & Maintenance
开机顺序:水槽升温、干燥达露点、配比空跑、挤出低速、测径标定、收卷上张力;停机反向走,先停料再停主机,模头不糊料。
Start-up runs water bath, dew point, dry dosing run, slow extrusion, gauge calibration, then winding tension; shut-down reverses it, stopping feed before the screw so the die stays clear.
参数速览 / Specifications
型号 TPD-1200|线径 1.75 与 2.85 mm|产能 30~120 kg/h|测径 双轴激光闭环|收卷 张力控制配排线|控制 PLC 配触控屏
Model TPD-1200 | 1.75 and 2.85 mm | 30-120 kg/h | Dual-axis laser gauging | Tension winding with traversing | PLC with touch panel
应用场景 / Applications
PLA、PETG、ABS、TPU 的单色与多色耗材量产,文创与教育耗材小批量试产,再生料掺混线的整线改造。
Volume production of single and multi-colour PLA, PETG, ABS and TPU filament, small creative and educational runs, and line retrofits for regrind blending.
选型与交付 / Sizing & Delivery
给出线径、色数、色段长度与小时产量四项即可出选型计算书,确认配置与产能;签约后按交期发运,到场安装、联动调试与操作培训,随机附手册与备件清单。
Send diameter, colour count, band length and hourly output for a sizing sheet that confirms configuration and capacity. After order we ship on the agreed date, install, commission and train, with manual and spare list.
常见问题 / FAQ
Q:整线一定要六段都配吗?
Q: Must all six stages be included?
A:不必。已有挤出机的客户可只配干燥、配比与测径收卷三段,按现有设备接口对接,投资更省。
No. Owners of existing extruders can take only drying, dosing and gauging with winding, interfacing to the machines already on site.
Q:线径波动先查哪一段?
Q: Which stage to check first for diameter wander?
A:先看测径曲线是慢漂还是周期性跳动:慢漂多为配比或温度,周期性跳动多为补料节拍与牵引同步。
Read the curve: slow drift points at dosing or temperature, while periodic jumps follow refill cycles and haul-off synchronisation.