PET注塑模具除露机之四

日期:2026-11-21 06:52
浏览次数:37
摘要:PET注塑模具除露机之四,PET瓶胚,PET注塑,模具除露机

PET注塑模具除露机之四,PET瓶胚,PET注塑,模具除露机


送风露点为设备额定核心参数,稳定在 - 40℃~-50℃且不可调,是实现除露的基础,若露点偏高则会导致气流带水汽,在冷模面形成二次凝露。
The supply air dew point is the rated core parameter of the equipment, stable at -40℃~-50℃ and non-adjustable, which is the basis for realizing dehumidification. If the dew point is too high, the air flow will carry water vapor and form secondary condensation on the cold mould surface.
送风温度根据设备类型可调,风冷式 40~60℃、水冷式 20~30℃、组合式 20~60℃,温度过高易导致模具升温、瓶胚冷却不充分,温度过低则会降低气流吸湿能力。
The supply air temperature is adjustable according to the equipment type, 40~60℃ for air-cooled type, 20~30℃ for water-cooled type, and 20~60℃ for combined type. Excessively high temperature is easy to cause mould heating and insufficient preform cooling, while excessively low temperature will reduce the moisture absorption capacity of the air flow.
送风风压调控范围为 0.05~0.3MPa,需根据模具腔数适配:48/96 腔中小腔数模具选 0.05~0.1MPa,144/288 腔大腔数模具选 0.1~0.2MPa,风压过低则吹扫无力,过高易吹损模具精密表面。
The supply air pressure regulation range is 0.05~0.3MPa, which needs to be adapted according to the number of mould cavities: 0.05~0.1MPa for small and medium cavity number moulds of 48/96 cavities, 0.1~0.2MPa for large cavity number moulds of 144/288 cavities. Too low air pressure results in weak purge, and too high air pressure is easy to damage the precision surface of the mould.
送风风速与风压联动,喷嘴出口风速 5~10m/s,气帘条出口 3~5m/s,喷嘴风速需保证吹走冷凝水,气帘条风速需保证形成稳定的阻隔气帘。
The supply air speed is linked with the air pressure, the wind speed at the nozzle outlet is 5~10m/s, and that at the air curtain strip outlet is 3~5m/s. The nozzle wind speed must ensure that the condensed water is blown away, and the air curtain strip wind speed must ensure that a stable barrier air curtain is formed.
吹扫时间 0.5~2s 可调,需与注塑开模时间匹配,单模周期 3~4s 选 0.5~1s,4~5s 选 1~2s,吹扫时间过短除露不彻底,过长则影响注塑合模节拍。
The purge time is adjustable from 0.5~2s, which needs to be matched with the injection mould opening time: 0.5~1s for a single mould cycle of 3~4s, 1~2s for 4~5s. Too short purge time results in incomplete dehumidification, and too long purge time affects the injection mould closing cycle.
设备通过工业级 PLC 实现所有工艺参数的闭环自动调控,传感器实时采集数据并反馈至控制系统,可自动修正温度、风压偏差,同时支持配方化管理,预存不同腔数模具的标准参数,一键调用即可。
The equipment realizes closed-loop automatic regulation of all process parameters through industrial PLC, the sensors collect data in real time and feed it back to the control system, which can automatically correct the temperature and air pressure deviation, and also support formula management, pre-storing standard parameters of moulds with different cavity numbers, which can be called with one key.
六、设备核心优势与应用价值
PET 注塑模具除露机从根源上消除模具凝露,可将凝露导致的瓶胚废品率从 3%~5% 降至 0.5% 以下,有效解决瓶胚发白、雾斑、缺料等外观缺陷,保障瓶胚成型品质。
PET injection mould dehumidifier eliminates mould condensation from the root cause, can reduce the preform scrap rate caused by condensation from 3%~5% to below 0.5%, effectively solve appearance defects such as preform whitening, foggy spots and material shortage, and ensure the forming quality of preforms.
设备与注塑机联动同步吹扫,无需停机除露,保障生产线 24h 连续运行,对于 288 腔等高速注塑生产线,产能提升幅度可达 15%~25%,大幅提高生产效率。
The equipment is connected with the injection moulding machine for synchronous purge without stopping the machine for dehumidification, ensuring the 24h continuous operation of the production line. For high-speed injection production lines such as 288 cavities, the production capacity can be increased by 15%~25%, greatly improving production efficiency.
干燥气流可有效阻隔凝露水与模具金属表面的接触,防止模具型腔、顶针、导柱等部件的锈蚀和磨损,延长模具使用寿命 30% 以上,降低模具维修和更换成本。
The dry air flow can effectively isolate the condensed water from contacting the metal surface of the mould, prevent the corrosion and wear of mould cavities, ejector pins, guide pillars and other components, extend the service life of the mould by more than 30%, and reduce the cost of mould maintenance and replacement.
设备采用变频风机、余热回收、联动吹扫等节能设计,相比传统除露方式能耗降低 60% 以上,同时结构紧凑,可壁挂 / 支架式安装,不占用车间宝贵的地面空间。
The equipment adopts energy-saving designs such as frequency conversion fan, waste heat recovery and interconnection purge, reducing energy consumption by more than 60% compared with traditional dehumidification methods, and has a compact structure, which can be installed on the wall/bracket without occupying valuable ground space in the workshop.
操作与维护门槛低,通过触摸屏即可完成所有操作,工艺参数配方化管理,无需专业技术人员;日常维护仅需定期清理过滤器、检查喷嘴,易损件更换周期明确,降低车间运维成本。
The threshold of operation and maintenance is low, all operations can be completed through the touch screen, the process parameters are managed in a formula way, and no professional technicians are needed; daily maintenance only needs to clean the filter and check the nozzle regularly, the replacement cycle of wearing parts is clear, reducing the workshop operation and maintenance cost.
设备可适配不同腔数、不同射速的 PET 瓶胚注塑生产线,吹扫单元支持定制化设计,同时可根据车间温湿度、生产需求选择不同温控类型,适配性极强。
The equipment can be adapted to PET preform injection production lines with different cavity numbers and different injection speeds, the purge unit supports customized design, and different temperature control types can be selected according to workshop temperature and humidity and production requirements, with extremely strong adaptability.